Stability limits of tin-based electrocatalyst supports

MPS-Authors
/persons/resource/persons136306

Geiger,  Simon
Electrocatalysis, Interface Chemistry and Surface Engineering, Max-Planck-Institut für Eisenforschung GmbH, Max Planck Society;

/persons/resource/persons188367

Kasian,  Olga
Electrocatalysis, Interface Chemistry and Surface Engineering, Max-Planck-Institut für Eisenforschung GmbH, Max Planck Society;

/persons/resource/persons125281

Mingers,  Andrea M.
Electrocatalysis, Interface Chemistry and Surface Engineering, Max-Planck-Institut für Eisenforschung GmbH, Max Planck Society;

/persons/resource/persons125274

Mayrhofer,  Karl J. J.
Helmholtz-Institute Erlangen-Nuremberg for Renewable Energy (IEK-11), Forschungszentrum Jülich, Egerlandstrasse 3, 91058 Erlangen, Germany;
Department of Chemical and Biological Engineering, Friedrich-Alexander-Universität Erlangen-Nürnberg, 91058 Erlangen, Germany ;
Electrocatalysis, Interface Chemistry and Surface Engineering, Max-Planck-Institut für Eisenforschung GmbH, Max Planck Society;

/persons/resource/persons125087

Cherevko,  Serhiy
Helmholtz-Institute Erlangen-Nuremberg for Renewable Energy (IEK-11), Forschungszentrum Jülich, Egerlandstrasse 3, 91058 Erlangen, Germany;
Electrocatalysis, Interface Chemistry and Surface Engineering, Max-Planck-Institut für Eisenforschung GmbH, Max Planck Society;

External Resource
No external resources are shared
Fulltext (restricted access)
There are currently no full texts shared for your IP range.
Fulltext (public)
There are no public fulltexts stored in PuRe
Supplementary Material (public)
There is no public supplementary material available
Citation

Geiger, S., Kasian, O., Mingers, A. M., Mayrhofer, K. J. J., & Cherevko, S. (2017). Stability limits of tin-based electrocatalyst supports. Scientific Reports, 7: 4595. doi:10.1038/s41598-017-04079-9.


Cite as: https://hdl.handle.net/11858/00-001M-0000-002D-A094-E
Abstract
Tin-based oxides are attractive catalyst support materials considered for application in fuel cells and electrolysers. If properly doped, these oxides are relatively good conductors, assuring that ohmic drop in real applications is minimal. Corrosion of dopants, however, will lead to severe performance deterioration. The present work aims to investigate the potential dependent dissolution rates of indium tin oxide (ITO), fluorine doped tin oxide (FTO) and antimony doped tin oxide (ATO) in the broad potential window ranging from -0.6 to 3.2 V-RHE in 0.1 M H2SO4 electrolyte. It is shown that in the cathodic part of the studied potential window all oxides dissolve during the electrochemical reduction of the oxide - cathodic dissolution. In case an oxidation potential is applied to the reduced electrode, metal oxidation is accompanied with additional dissolution - anodic dissolution. Additional dissolution is observed during the oxygen evolution reaction. FTO withstands anodic conditions best, while little and strong dissolution is observed for ATO and ITO, respectively. In discussion of possible corrosion mechanisms, obtained dissolution onset potentials are correlated with existing thermodynamic data.