Deutsch
 
Hilfe Datenschutzhinweis Impressum
  DetailsucheBrowse

Datensatz

DATENSATZ AKTIONENEXPORT

Freigegeben

Zeitschriftenartikel

Thermal properties of thermoplastic polymers: Influence of polymer structure and procedure of radical polymerization

MPG-Autoren
/persons/resource/persons133766

Wei,  Chunxiang
Klaus Tauer, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

/persons/resource/persons121270

Esposito,  Davide
Davide Esposito, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

/persons/resource/persons121928

Tauer,  Klaus
Klaus Tauer, Kolloidchemie, Max Planck Institute of Colloids and Interfaces, Max Planck Society;

Externe Ressourcen
Es sind keine externen Ressourcen hinterlegt
Volltexte (beschränkter Zugriff)
Für Ihren IP-Bereich sind aktuell keine Volltexte freigegeben.
Volltexte (frei zugänglich)
Es sind keine frei zugänglichen Volltexte in PuRe verfügbar
Ergänzendes Material (frei zugänglich)
Es sind keine frei zugänglichen Ergänzenden Materialien verfügbar
Zitation

Wei, C., Esposito, D., & Tauer, K. (2016). Thermal properties of thermoplastic polymers: Influence of polymer structure and procedure of radical polymerization. Polymer Degradation and Stability, 131, 157-168. doi:10.1016/j.polymdegradstab.2016.07.016.


Zitierlink: https://hdl.handle.net/11858/00-001M-0000-002B-1A0E-0
Zusammenfassung
Experimental data prove a significant mutual interference between the chemical nature of the monomer and the particularities of the radical polymerization procedure which influences the thermal decomposition (depropagation) of the corresponding polymer. Results are presented for polystyrene, poly(methyl methacrylate), and poly(α-methylene-γ-valerolactone) which were made via different radical polymerization techniques (thermally self-initiated bulk polymerization at 80 °C, photoinitiated bulk and aqueous heterophase polymerization at 25 °C). Also, experimental data are presented after thermally annealing the polymers at 200 and 300 °C.