English
 
Help Privacy Policy Disclaimer
  Advanced SearchBrowse

Item

ITEM ACTIONSEXPORT

Released

Journal Article

Investigation of hydrogen discharging and recharging processes of Ti-doped NaAlH4 by X-ray diffraction analysis (XRD) and solid-state NMR spectroscopy

MPS-Authors

Bogdanović,  B.
Research Group Bogdanović, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons58541

Felderhoff,  M.
Research Department Schüth, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons58570

Germann,  M.
Research Department Schüth, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons58605

Härtel,  M.
Research Department Schüth, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons58895

Pommerin,  A.
Research Department Schüth, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons58985

Schüth,  F.
Research Department Schüth, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons59100

Weidenthaler,  C.
Research Department Schüth, Max-Planck-Institut für Kohlenforschung, Max Planck Society;

/persons/resource/persons59145

Zibrowius,  B.
Service Department Mynott (NMR), Max-Planck-Institut für Kohlenforschung, Max Planck Society;

External Resource
No external resources are shared
Fulltext (restricted access)
There are currently no full texts shared for your IP range.
Fulltext (public)
There are no public fulltexts stored in PuRe
Supplementary Material (public)
There is no public supplementary material available
Citation

Bogdanović, B., Felderhoff, M., Germann, M., Härtel, M., Pommerin, A., Schüth, F., et al. (2003). Investigation of hydrogen discharging and recharging processes of Ti-doped NaAlH4 by X-ray diffraction analysis (XRD) and solid-state NMR spectroscopy. Journal of Alloys and Compounds, 350(1-2), 246-255. doi:10.1016/S0925-8388(02)00953-2.


Cite as: https://hdl.handle.net/11858/00-001M-0000-000F-98B3-F
Abstract
The processes occurring in the course of two sequential hydrogen discharging and recharging cycles of Ti-doped sodium alanate were investigated in parallel using XRD analysis and solid-state NMR spectroscopy. Both methods demonstrate that in hydrogen storage cycles (Eq. (1)) the majority phases involved are NaAlH4, Na3AlH6, Al and NaH. Only traces of other, as yet unidentified phases are observed, one of which has been tentatively assigned to an Al–Ti alloy on the basis of XRD analysis. The unsatisfactory hydrogen storage capacities heretofore observed in cycle tests are shown to be due entirely to the reaction of Na3AlH6 with Al and hydrogen to NaAlH4 (Eq. (1), 2nd hydrogenation step) being incomplete. Using XRD and NMR methods it has been shown that a higher level of rehydrogenation can be achieved by adding an excess of Al powder.